CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROCARB
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural elements, and insulating components. Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.080 %
0.080 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 150 MPa
21800 psi
value at 30 sec.; ISO 2039-1
Tensile Strength at Break 55.0 MPa
7980 psi
v = 5 mm/min; ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-2
Flexural Modulus 4.70 GPa
682 ksi
ISO 178
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C
248 °F
Long Term
140 °C
284 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ISO 75-2
Vicat Softening Point 148 °C
298 °F
VST/B/50; ISO 306
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
V-2

@Thickness 6.00 mm
V-2

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 60093
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
IEC 60250
3.6

@Frequency 100 Hz
3.6

@Frequency 100 Hz
IEC 60250
Dielectric Strength 36.0 kV/mm
914 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.0080

@Frequency 1e+6 Hz
0.0080

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V
175 V
IEC 60112