CENTROPLAST CENTROLEN PP LF Polypropylene conductive

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROLEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROLEN PP LF Polypropylene conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is a low density, easily machined plastic that can be welded and has good surface conductivity. Applications include filter heads and housings, conveyor equipment for flammable liquids, and pump bodies for mining.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption at Saturation <= 0.20 %
<= 0.20 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Tensile Modulus 1.45 GPa
210 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 3.20 J/cm²
15.2 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Electrical Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
IEC 60093
Surface Resistance <= 1000 ohm
<= 1000 ohm
IEC 60093