Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 30% Glass Filled
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROPHEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.060 %
0.060 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 MPa
18900 psi
value at 30 sec.; ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
v = 5 mm/min; ISO 527-2
Elongation at Break 1.5 %
1.5 %
ISO 527-2
Tensile Modulus 8.00 GPa
1160 ksi
ISO 527-2
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 - 1.00 J/cm²
3.81 - 4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Melting Point 290 °C
554 °F
10K/min; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ISO 75-2
Vicat Softening Point 145 °C
293 °F
VST/B/50; ISO 306
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 1e+6 Hz
0.0010

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved