Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROPHEN Polyphenylene ether modified

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROPHEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROPHEN Polyphenylene ether modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include fittings, drive components for domestic appliances, and components for electrotechnical equipment.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.060 %
0.060 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.23 %
0.23 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 100 MPa
14500 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 55.0 MPa
7980 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 30 %
30 %
ISO 527-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
Melting Point 290 °C
554 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 90.0 °C
194 °F
Long Term
105 °C
221 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ISO 75-2
Vicat Softening Point 135 °C
275 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 2.7

@Frequency 1e+6 Hz
2.7

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm
483 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 1e+6 Hz
0.0010

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V
175 V
IEC 60112
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes
FD A
Users viewing this material also viewed the following: