CIMBAR CIMBAR™ BF Barite Powder (BaSO4)

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name CIMBAR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR CIMBAR™ BF Barite Powder (BaSO4).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CIMBAR Performance Minerals BF product is the next generation of precipitated extenders. With its micro-fine particle size, high barium sulfate content, low solubility, high brightness and chemical inertness, BF is ideal for applications such as topcoats, printing inks, powder coatings and lead-acid batteries as well as many others. Cimbar BF has excellent gloss, dispersability and weather resistance. Uses:PlasticsArchitectural coatingsBatteriesCosmeticsPharmaceuticalsAutomotive PrimersAutomotive TopcoatsGloss EnamelsPowder CoatingsSemi-gloss LatexesIndustrial CoatingsInformation provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 4.40 g/cc
4.40 g/cc
Fineness 8.0
8.0
Hegman Fineness
Particle Size 0.68 µm
0.68 µm
mean
pH 8.0
8.0
Mechanical Properties Metric English Comments
Hardness, Mohs 3.0
3.0
Optical Properties Metric English Comments
Refractive Index 1.64
1.64
Descriptive Properties Value Comments
BaSO4 (%) 99
Color-a -0.32
Color-b 0.84
Color-L 99.3
Color-Z 97.3
Paint Coating Gloss (20/60) 59.0/89.8
Paint Viscosity (10/100) 1010/530