Material Notes:
The 200 series consists of PTFE/polyester combination fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated polymer material made by impregnating textile with a thermoset resin. CIP Composites™ offer design engineers an attractive, cost effective alternative to the traditional materials used for bushings, bearings, wear pads, and thrust washers, such as bronze, brass or nylon. CIP Composites™ are only 1/6 the weight of steel, easily machined, have good dimensional stability and do not contain harmful or toxic materials.
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.0500 - 0.09
0.0500 - 0.09
Dry, Grade CIP 251 (MoS2 + PTFE Filled)
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 20.0 - 93.3 °C
17.8 µin/in-°F

@Temperature 68.0 - 200 °F
Parallel to Laminate
CTE, linear, Transverse to Flow 63.0 µm/m-°C

@Temperature 20.0 - 93.3 °C
35.0 µin/in-°F

@Temperature 68.0 - 200 °F
Normal to Laminate
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F