CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer CMW Inc.
Trade Name ELKALOY
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKALOY D110 Copper Alloy, Aluminum Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility.ELKALOY® D110 material is recommended for butt and flash welding dies and clamps for applications similar to ELKALOY® D material but requiring higher strength. ELKALOY® D110 material is used for structural current carrying members for welding die fixtures in samples similar to those for ELKALOY® D material. In addition, ELKALOY® D110 material is good for use as bearings, slides and gibbs in contact with steel. Due to its low coefficient of friction with steel and due to its good corrosion resistance, it is also used for valve stems, seats and wedges.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 7.50 g/cc
0.271 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 88
88
Tensile Strength, Ultimate 621 MPa
90100 psi
Tensile Strength, Yield 262 MPa
38000 psi
Elongation at Break 12 %
12 %
Reduction of Area 12 %
12 %
Modulus of Elasticity 97.0 GPa
14100 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 100 °C
10.0 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 75.0 W/m-K
521 BTU-in/hr-ft²-°F
Melting Point 1025 - 1060 °C
1877 - 1940 °F
Solidus 1025 °C
1877 °F
Liquidus 1060 °C
1940 °F
Component Elements Properties Metric English Comments
Aluminum, Al 10.8 %
10.8 %
Beryllium, Be 0.50 %
0.50 %
Co + Ni 1.5 - 2.55 %
1.5 - 2.55 %
Copper, Cu 82.55 - 83.6 %
82.55 - 83.6 %
Iron, Fe 3.6 %
3.6 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000144 ohm-cm
0.0000144 ohm-cm
12 % IACS