Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKON 100M Pure Molybdenum

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal , Pure Element
Manufacturer CMW Inc.
Trade Name ELKON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKON 100M Pure Molybdenum.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The electrical and thermal conductivity of the two metals is essentially the same. It is fabricated into electrical contacts by slicing discs from rods and brazing them to nickel-plated steel backings, which may be in the form of rivets, screws, or stampings. In atmospheres of inert gasses or vacuum, molybdenum contacts can handle currents of several amperes. Here it has good resistance to welding and electrical erosion because of its refractory metal characteristics. It is readily wet by mercury to form a low resistance contact and is used extensively in mercury switches. It does not contaminate the mercury because it does not react chemically with it. Molybdenum oxidizes more readily than tungsten and, therefore, is seldom used in air applications. If used in air, it is generally limited to 1 ampere and several hundred volts. In certain vibrating contact applications, low mass contacts are desirable, and molybdenum is selected because of its low density. Because of its low expansion characteristic, it is used in non-contact applications such as bases for semiconductor devices. It is also used for faces on resistance welding electrodes.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.22 g/cc
0.3692 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 58
58
Tensile Strength, Ultimate 585 MPa
84800 psi
Modulus of Elasticity 324 GPa
47000 ksi
Thermal Properties Metric English Comments
CTE, linear 5.35 µm/m-°C

@Temperature 100 °C
2.97 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 142 W/m-K
985 BTU-in/hr-ft²-°F
Melting Point 2622 °C
4752 °F
Boiling Point 4800 °C
8670 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 100 %
100 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000520 ohm-cm
0.00000520 ohm-cm
33 % IACS
Users viewing this material also viewed the following: