Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONITE® 1060 Silver Tungsten Carbide Contact Material

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® 1060 Silver Tungsten Carbide Contact Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrical contactor material for medium current ac applicationsInformation provided by CMW Inc.
Physical Properties Metric English Comments
Density 12.83 g/cc
0.4635 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 102
102
Flexural Modulus 0.827 GPa
120 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 260 W/m-K
1800 BTU-in/hr-ft²-°F
Melting Point >= 980 °C
>= 1800 °F
Solidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
Cobalt, Co 1.5 %
1.5 %
Silver, Ag 40 %
40 %
WC 58.5 %
58.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000475 ohm-cm
0.00000475 ohm-cm
(36% IACS)
Users viewing this material also viewed the following: