Material Notes:
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting point (1552(C) and, like platinum, resists arc formation. Its low electrical conductivity (16% IACS) limits its application to low current circuits. It costs much less than platinum, and is used as a lower cost alternative. Economics normally dictate that it be supplied as a composite contact with a thin contact metal facing silver brazed to a nickel-plated steel rivet, screw, or projection weld button backing.ELKONIUM® 40 is CMW's trademark for commercially pure palladium (9.90 minimum purity). Its good corrosion resistance and low hardness makes it a desirable contact for low current applications where forces are relatively low and reliability of making circuit is important. It is used in aircraft relays at currents under 1 ampere, in telephone relays and in instruments. It is often chosen for applications where contacts area open for long periods of time.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 12.0 g/cc
0.434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 57
57
annealed
82
82
cold worked
Tensile Strength, Ultimate 193 MPa
28000 psi
annealed
324 MPa
47000 psi
cold worked
Elongation at Break 5.0 %
5.0 %
cold worked
28 %
28 %
annealed
Component Elements Properties Metric English Comments
Palladium, Pd >= 99.9 %
>= 99.9 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000108 ohm-cm
0.0000108 ohm-cm
16 % IACS