Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer CP-Polymer-Technik GmbH & Co.
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by CP-Polymer-Technik GmbH & Co. KG
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.0 - 2.5 %
2.0 - 2.5 %
23°C/50%RH; DIN 53495
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 4.00 mm
0.0020 in/in

@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Thickness 4.00 mm
0.0070 in/in

@Thickness 0.157 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
5 mm/min; ISO 527
Elongation at Break 3.5 %
3.5 %
5 mm/min; ISO 527
Tensile Modulus 8.20 GPa
1190 ksi
ISO 527
Flexural Modulus 7.40 GPa
1070 ksi
DIN 52457
Charpy Impact Unnotched 6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
Melting Point 255 °C
491 °F
Kofler
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 179
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 179
Vicat Softening Point 230 °C
446 °F
50 N; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Stufe; IEC 707
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Stufe; IEC 707
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
ISO 3915
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 40.0 kV/mm
1020 kV/in
IEC 243-1
Dielectric Loss Index 0.015
0.015
At 1 MHz; IEC 250
Comparative Tracking Index 550 V
550 V
Stufe; IEC 112
Processing Properties Metric English Comments
Melt Temperature 265 - 295 °C
509 - 563 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Descriptive Properties Value Comments
Back Pressure Low
Holding Pressure High
Injection Speed High
Screw Speed Medium
Users viewing this material also viewed the following: