CPT C-Flex® R70-026 Opaque Biocompatible TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Consolidated Polymer Technologies
Trade Name C-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPT C-Flex® R70-026 Opaque Biocompatible TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current United States Pharmacopoeia Class VI test requirements. C-Flex® does not contain latex rubber, polyvinyl chloride, silicone rubber, or polyurethane.Information provided by Consolidated Polymer Technologies.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D 792
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
Melt Flow 11.7 g/10 min
11.7 g/10 min
Condition D; ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
1 sec.; ASTM D 2240
Tensile Strength at Break 10.98 MPa
1593 psi
ASTM D 412
Elongation at Break 461 %
461 %
ASTM D 412
100% Modulus 0.00696 GPa
1.01 ksi
ASTM D 412
300% Modulus 0.00807 GPa
1.17 ksi
ASTM D 412
Tear Strength 70.8 kN/m
404 pli
Die C; ASTM D 624
71.7 kN/m
409 pli
Notched, Die B; ASTM D 624
Taber Abrasion, mg/1000 Cycles 124.6
124.6
Federal Test Method Standard, 405
Compression Set 50 %
50 %
23°C; ASTM D 412
74 %

@Temperature 70.0 °C
74 %

@Temperature 158 °F
ASTM D 412
Tensile Set 148 %
148 %
at 300% elongation; ASTM D 412
185 %
185 %
at break; ASTM D 412
Processing Properties Metric English Comments
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
Descriptive Properties Value Comments
Sterilization methods: Steam/Autoclave, Ethylene Oxide
Cobalt 60 not recommended