Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cadi 100M Molybdenum

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal , Pure Element
Manufacturer Cadi Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cadi 100M Molybdenum.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 10.2 g/cc
0.368 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 89
89
Component Elements Properties Metric English Comments
Molybdenum, Mo 100 %
100 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000573 ohm-cm
0.00000573 ohm-cm
Calculated from 30 %IACS
Descriptive Properties Value Comments
RMWA Class 14
Copyright © lookpolymers.com All Rights Reserved