Material Notes:
General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at high temperatures. It is tough and ductile at sub-zero temperatures.C 200 is ferromagnetic and has one of the largest magnetostrictive effects of any commercial material. Its thermal and electrical conductivities are considerably higher than other stainless steels of nickel alloys.Carlson C 201 is a restricted carbon (0.02% max.) version of C 200. It is preferred for exposure to temperatures above 600°F (315°C); and it is superior whenever creep strength is an important criterion.ApplicationsC200 and C 201 provide excellent corrosion resistance to hot concentrated alkali (except ammonium hydroxide). These alloys exhibit good corrosion resistance to dry chlorine, fluorine, hydrogen chloride and hydrogen fluoride up to moderately elevated temperatures.The corrosion resistance of both alloys make them particularly useful for maintaining product purity in food processing and in the production or processing of synthetic fibers, alkalis, fatty acids, soaps and detergents.Chemical Processing – caustic processing and storage, chemical shipping containers, synthetic fiber productions, fluorine electrolysis.Food Processing EquipmentMagnetostructive DevicesAerospace and Missile components – rocket motor cases.Information provided by Carlson
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 379 MPa
>= 55000 psi
Tensile Strength, Yield >= 82.7 MPa

@Strain 0.200 %
>= 12000 psi

@Strain 0.200 %
Elongation at Break >= 40 %
>= 40 %
Modulus of Elasticity 193 GPa
28000 ksi
Tension
Poissons Ratio 0.29
0.29
Shear Modulus 75.2 GPa
10900 ksi
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 27.0 - 100 °C
7.22 µin/in-°F

@Temperature 80.6 - 212 °F
Specific Heat Capacity 0.4535 J/g-°C

@Temperature 0.000 °C
0.1084 BTU/lb-°F

@Temperature 32.0 °F
Thermal Conductivity 60.7 W/m-K

@Temperature 27.0 - 100 °C
420 BTU-in/hr-ft²-°F

@Temperature 80.6 - 212 °F
Melting Point 1435 - 1446 °C
2615 - 2635 °F
Solidus 1435 °C
2615 °F
Liquidus 1446 °C
2635 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.020 %
<= 0.020 %
Copper, Cu <= 0.25 %
<= 0.25 %
Iron, Fe <= 0.40 %
<= 0.40 %
Manganese, Mn <= 0.35 %
<= 0.35 %
Nickel, Ni >= 99 %
>= 99 %
Silicon, Si <= 0.35 %
<= 0.35 %
Sulfur, S <= 0.010 %
<= 0.010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000118 ohm-cm
0.0000118 ohm-cm
Curie Temperature 360 °C
680 °F