Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® Y 50 V Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® Y 50 V Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAPILENE® Y 50 V is an ultra high melt flow rate polypropylene homopolymer suitable for thin walled injection molding and as a base resin for compounds applications. The product combines high stiffness, low warpage and good dimensional stability. APPLICATIONS CAPILENE ® Y 50 V is designed for thin walled injection molding packaging and compounds applications.
Physical Properties Metric English Comments
Melt Flow 120 g/10 min

@Load 2.16 kg,
Temperature 230 °C
120 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 0.170 J/cm

@Temperature >=23.0 °C
0.318 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Vicat Softening Point 150 °C

@Load 1.02 kg
302 °F

@Load 2.25 lb
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved