Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® AC125 Acetal Copolymer, 25% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® AC125 Acetal Copolymer, 25% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Glass fiber reinforcedAlkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantResilientHigh rigiditySolvent resistantHigh strengthGood thermal stabilityGood toughnessForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Filler Content 25 %
25 %
Water Absorption 0.26 %
0.26 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
0.125 in; ASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength, Yield 114 MPa
16500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
0.125 in; ASTM D256
Tensile Impact Strength 94.5 kJ/m²
45.0 ft-lb/in²
Type S; ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 166 °C
330 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
322 °F
Unannealed; ASTM D648