Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Filler Content 40 %
40 %
Water Absorption 0.90 %
0.90 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
0.125 in; ASTM D256
Tensile Impact Strength 147 kJ/m²
70.0 ft-lb/in²
Type S; ASTM D1822
Thermal Properties Metric English Comments
Melting Point 216 - 220 °C
420 - 428 °F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Unannealed; ASTM D648