Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN100M2 (Dry) Nylon 66, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN100M2 (Dry) Nylon 66, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good chemical resistanceFast cycleDurableLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 7.5 %
7.5 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: