Chase Plastics CP Pryme® NN130M2 (Dry) Nylon 66, 30% Glass Fiber Reinforced, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN130M2 (Dry) Nylon 66, 30% Glass Fiber Reinforced, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good chemical resistanceGood compressive strengthGood creep resistanceFast cycleLubricatedHigh rigiditySolvent resistanceHigh strengthForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.60 %
0.60 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 148 MPa
21500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F