Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good flowHigh rigidityGood toughnessHigh strengthLow viscosityGood mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Appearance Opaque, Transparent