Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 100 W Nylon 66, MoS2 Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 100 W Nylon 66, MoS2 Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A molybdenum disulfide modified nylon 66 exhibiting superior tensile strength and wear resistance, greater dimensional stability and higher heat resistance than general purpose nylon 66.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 94.0 MPa
13600 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Yield Strength 121 MPa
17500 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 271 °C
520 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved