Material Notes:
A 4 melt flow index copolymer acetal for extrusion or thick injection molding applications.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
MFI condition not specified
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 190 °C
374 °F