Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic SW02 POM/PTFE

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, PTFE Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic SW02 POM/PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 83
83
ASTM D785
Tensile Strength, Yield 57.9 MPa
8390 psi
ASTM D638
Flexural Yield Strength 93.2 MPa
13500 psi
ASTM D790
Izod Impact, Notched 0.804 J/cm
1.51 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: