Chengdu Polyster 75 LPI Lenticular Lens Sheet, APET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster 75 LPI Lenticular Lens Sheet, APET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The thickness is moderate. It is good for ink adhesion, and specially designed for advertisement and packing. It is one of the lenticular lens sheets used widely, such as packaging bags, gift boxes, hang hag, stationaries, postcards, posters, books and other beautiful promotion items. The suitable graphic effects: flip, 3D, animation, morph, zoom, moire, etc.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Thickness 11.4 microns
0.450 mil
15.2 microns
0.600 mil
Storage Temperature 23.0 - 30.0 °C
73.4 - 86.0 °F
Descriptive Properties Value Comments
Lenses Per Inch (LPI) 75
Optimum Storage Humidity (%) 70
Viewing Angle (°) 49
Viewing Distance (m) 0.15 to 1.8