Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Melt Flow 5.0 - 10 g/10 min
5.0 - 10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
ISO 868
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ISO 527-1
Elongation at Break 400 %
400 %
ISO 527-1
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Tear Strength 40.0 kN/m
228 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 156 °C
313 °F
ISO 3146
Brittleness Temperature -50.0 °C
-58.0 °F
ISO 974