Chengdu Polyster H2040 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H2040 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Like H4040, except that heat-ageing resistance is improved. Applications requiring better heat-ageing resistance.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Melt Flow 7.0 - 9.0 g/10 min
7.0 - 9.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ISO 868
Tensile Strength, Ultimate 25.0 MPa
3630 psi
ISO 527-1
Elongation at Break 530 %
530 %
ISO 527-1
Flexural Modulus 0.0560 GPa
8.12 ksi
ISO 178
Tear Strength 91.0 kN/m
519 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 190 °C
374 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974