Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Melt Flow 10 - 15 g/10 min
10 - 15 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 30
30
ISO 868
Tensile Strength, Ultimate 14.0 MPa
2030 psi
ISO 527-1
Elongation at Break 550 %
550 %
ISO 527-1
Flexural Modulus 0.0280 GPa
4.06 ksi
ISO 178
Tear Strength 50.0 kN/m
285 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974
Copyright © lookpolymers.com All Rights Reserved