Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H3303B Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H3303B Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low modulus molding and extrusion grade. Contains color-stable antioxidants. Excellent low-temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ boots, hose jackets, wire and cable jackets, film and sheeting, belting, profiles and seals, etc.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Melt Flow 0.50 - 1.5 g/10 min
0.50 - 1.5 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
ISO 868
Tensile Strength, Ultimate 18.0 MPa
2610 psi
ISO 527-1
Elongation at Break 400 %
400 %
ISO 527-1
Flexural Modulus 0.0400 GPa
5.80 ksi
ISO 178
Tear Strength 100 kN/m
571 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974