Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H605B Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H605B Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Good melt stability. CVJ boots, dust cover, bellows, jackets and air ducts of engine, etc.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 0.50 - 1.5 g/10 min
0.50 - 1.5 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ISO 868
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ISO 527-1
Elongation at Break 350 %
350 %
ISO 527-1
Flexural Modulus 0.156 GPa
22.6 ksi
ISO 178
Tear Strength 163 kN/m
930 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 196 °C
385 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974