Chengdu Polyster H8570Y Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H8570Y Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High modulus molding and injection grade. Contains improved color- stable antioxidants. Low frictional coefficient and good abrasion resistance. Applications requiring high strength, high toughness good abrasion resistance and good properties at high temperature.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Melt Flow 7.0 - 10 g/10 min
7.0 - 10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ISO 868
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ISO 527-1
Elongation at Break 350 %
350 %
ISO 527-1
Flexural Modulus 0.600 GPa
87.0 ksi
ISO 178
Tear Strength 200 kN/m
1140 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 3146
Brittleness Temperature -50.0 °C
-58.0 °F
ISO 974