Chengdu Polyster KLX-G11 PC Film & Sheet

Category Polymer , Film , Thermoplastic , Polycarbonate (PC)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster KLX-G11 PC Film & Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant, sunglass, sunbonnet, electroplate, .Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
23 to 24 hours; ASTM D570
Thickness 3.17 - 25.4 microns
0.125 - 1.00 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D2240
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ASTM D882
Elongation at Break 140 %
140 %
ASTM D882
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Izod Impact, Notched 7.00 - 8.60 J/cm
13.1 - 16.1 ft-lb/in
Izod tape gap; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM D117
Maximum Service Temperature, Air 110 °C
230 °F
Flammability, UL94 V-2

@Thickness 0.400 mm
V-2

@Thickness 0.0157 in
Shrinkage 0.50 - 0.70 %
0.50 - 0.70 %
Optical Properties Metric English Comments
Refractive Index 1.585
1.585
ASTMD542
Haze 3.0 %

@Thickness 1.00 mm
3.0 %

@Thickness 0.0394 in
ASTMD1003
Transmission, Visible 89 %

@Thickness 1.00 mm
89 %

@Thickness 0.0394 in
ASTMD1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Strength 30.0 kV/mm

@Thickness 1.60 mm
762 kV/in

@Thickness 0.0630 in
ASTM D149
Arc Resistance 110 sec

@Frequency 1.00e+6 Hz
110 sec

@Frequency 1.00e+6 Hz
ASTM D495