Chengdu Polyster KP-200-40 Silicone Masterbatch

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Silicone
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster KP-200-40 Silicone Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KP-200 series silicone masterbatches are white pellets or white powder which made from ultra-high molecular weight polysiloxane, used by plastics as processing aids and impart expected silicone benefits to plastics, often more efficiently and more effectively than lower molecular weight silicone fluids, such as safety, little effect on the adhesion of paints, labels or decorations, more convenient to handle, good dispersion. Silicone masterbatches are with the carrier of polyethylene. For KP-200-30 silicone masterbatch, the content of siloxane is 30%. For KP-200-40 silicone masterbatch, the content of siloxane is 40%. For KP-200-50 silicone masterbatch, the content of siloxane is 50%. KP-200H silicone masterbatch is 100% pure silicone powder. KP-200 silicone masterbatch is with special silicon powder carrier, the content of silicone with ultra-high molecular weight is 50%.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
GB/T 3682
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.0 MPa
3340 psi
GB/T1040-1992
Elongation at Break 730 %
730 %
GB/T1040-1992
Coefficient of Friction 0.15
0.15
coefficient of inner wall; GB/T3960-83
Component Elements Properties Metric English Comments
Silicon, Si 40 %
40 %