Chesterton 274 Industrial Degreaser

Category Fluid , Solvent
Manufacturer Chesterton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 274 Industrial Degreaser.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 274 Industrial Degreaser is an industrial strength, hard surface degreaser which will dissolve grease, oil, tar and other similar water insoluble soils generally encountered in industrial and marine environments. Industrial Degreaser is designed to be used as received and may be applied by spray, brush or dipping. It is commonly used in commercial parts washers to replace more hazardous solvents. Chesterton 274 Industrial Degreaser has a high flash point and low aromatic content. It offers greatly improved safely compared to conventional petroleum based degreasers. Features:Dissolves Grease, Oil, Tar and Other Organic SoilsHigh Flash PointLow Aromatic ContentLow OdorLow Evaporation Rate Does Not Attack Most Paints and PlasticsSafe For Use on All MetalsFast Penetrating ActionNSF C1, K1, K2 Registration number 133955 (bulk) and 133949 (aerosol)Suggested Uses:Degreasing metal parts, equipment, vehicles, floors and other hard surfacesReplacement for kerosene, mineral spirits, chlorinated solvents and naphtha based cleaners and degreasersUse in recirculating and agitated parts washers and dip tanksDegrease surfaces prior to coatingClean equipment before disassembly for maintenance, repair, or machiningRemove process oils and other contaminates from in process partsApplications can be found in metal production operations, paint ships, maintenance departments, boiler rooms, repair shops, vehicle and ship yards, among othersCleans non-energized electrical equipment.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.780 g/cc
0.780 g/cc
Volatiles 100 %
100 %
Vapor Pressure <= 0.0133 bar
<= 10.0 torr
ASTM D2879
Thermal Properties Metric English Comments
Flash Point 62.0 °C
144 °F
Tag Closed Cup; ASTM D56
Electrical Properties Metric English Comments
Dielectric Strength 1.97 kV/mm
50.0 kV/in
ASTM D877
Descriptive Properties Value Comments
Appearance Clear, transparent liquid
Aromatic Content <0.2%
(C8+)
Auto-ignition temperature 227°C
ASTM D2155
Color, Saybolt >30
ASTM D156
Evaporation Rate 151
n-Butyl Acetate=1