Chesterton 438 PTFE Coating

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Chesterton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 438 PTFE Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 438 PTFE Coating represents the best combination of clean, dry, PTFE – based powder lubricant with a tough, protective coating that resists water and chemicals. It does much more than simply reduce friction; the product actually coats and protects the surfaces of parts and equipment. 438 PTFE Coating effectively lubricates and protects smooth, nonporous surfaces, including metal, plastic, wood, leather, fiber, rubber, glass and painted surfaces. It will not rub, wipe or run off like liquid lubricants can, nor will it collect dirt and grime as grease lubricants are prone to do. It dries instantly; leaving no waxy or oily film that can stain and attract dirt particles, therby eliminating quality control losses from stained or damaged products and packaging. The coating resists water washout, as well as mild acids and alkalies, thus reducing the number of applications necessary to maintain functionality. Because 438 PTFE Coating makes the surface of parts and equipment extremely slippery, the product is ideal for coating inner surfaces of hoppers, bins, slides and anywhere else adherence of material is a problem. Applying the coating to these surfaces eliminates hangups and costly production stoppages. When several coats are applied, the product provides long-lasting surface protection and helps resist abrasive wear.Features:Contains ultra-fine PTFE particlesSlippery; low coefficient of frictionDry, non-oily, non-greasyClean, nonstainingSpecifically designed for smooth, nonporous surfacesExcellent chemical resistanceStrong resistance to washoutWill not absorb or hold moistureNSF H2 – Registration number 133951 (bulk) and 13395 (aerosol)Benefits:Stop sticking and material buildupSignificantly reduce power consumptionProlong the life of machinery and partsSave the cost of replacement partsReduce lubricant costsReduce maintenance costsSave production timeApplications: 438 PTFE Coating, a versatile, long-lasting PTFE powder reinforced film, protects all types of smooth, nonporous surfaces, including metal, plastics, wood, leather, fiber, elastomers, glass and painted surfaces. It can be used on instruments, machine tools, conveyor belts, bearings, cold molds, dies, and even drawers and windows. When used to coat inner surfaces of bins, tanks, hoppers, molds and slides, the lubricant helps prevent materials from adhering, thus avoiding hangups and production stoppage. It is excellent for paper converting equipment to stop the paper from shifting as it is folded.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.850 g/cc
0.850 g/cc
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Descriptive Properties Value Comments
Appearance Dry, white powder in clear film
Base Pure PTFE powder