Chesterton 995 Release Agent

Category Fluid , Lubricant , Silicone Base
Manufacturer Chesterton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 995 Release Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 995 Release Agent is a highly effective release agent free of all chlorinated solvents. Environmental responsibility need not mean a compromise on performance. Chesterton 995 Release Agent will give maximum release without sticking, spotting or marking. Chesterton 995 is formulated for use in all mold applications ranging from sand core operations and investment casting to hard-to-release molding procedures with polyurethanes, rubber, filled thermoplastics and composites. Chesterton 995 Release Agent will aid in the production of clean pieces with high gloss surfaces. It will give immediate release with no deformation. 995 will prevent sticking on straight sides or tearing of thin sections. Orange peel and blisters will be virtually eliminated. Chesterton 995 is concentrated. Multiple releases are possible with one application from molds of aluminum, steel etc., cast, compression or injection. Production rates and return on investment are maximized as fewer applications are necessary. Effectiveness of Chesterton 995 compared to other mold releases can be measured easily by operators. Independent laboratory results showed Chesterton 995 Release Agent gave approximately 20% more releases per application than other nationally recognized release agents and showed less build-up in the test molds.Features:Superior Silicone BaseNo Chlorinated Solvents, Freons (CFC's), or Halogenated CompoundsNo mold build-upBenefitsHIgh gloss, wet look finishMultiple releasesLeaves molds cleanerFewer rejectsFiner detailFaster cyclingEasily appliedSuggested Uses:Molding MethodsSand Core OperatingInvestment CastingInjection MoldingThermosetsThermoplasticsAluminum DiecastingZinc DiecastingMaterials MoldedAcrylic Cellulosic(s)PolystyrenePolyesterPolyurethaneRubberActive ingredient: Complexe Silicone Release AgentInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.743 g/cc
0.743 g/cc
Descriptive Properties Value Comments
Appearance Thin film, Liquid
Color Clear, Colorless
Users viewing this material also viewed the following: