Material Notes:
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sagging, non-shrinking, and 100% solids. The ARC 10 is formulated for applications where machining to exact tolerances is required or desired. It is frequently used as an alternative to resurfacing by welding or flame spraying. ARC 10 is easily mixed and applied and cures without the need of heat or pressure. Benefits:High build characteristic allow for single coat applicationsTough resin structure resist thermal-mechanical shockOutstanding adhesion insures reliable performanceCan be easily machined to exact tolerancesConvenient 4-1 mix ratio and verification of mix by color changePerforms well under fluctuating chemical environmentsResists compression setting. Suggested Uses:Condensersli>Cooling Water PumpsFlange FacesHydraulic RamsKeywaysValve BodiesBearing HousingsShaftsSpline RepairsPitted CastingsHeat ExchangersPump Volutes Information provided by Chesterton
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Taber Abrasion, mg/1000 Cycles 275

@Load 0.250 kg
275

@Load 0.551 lb
H-18/250g; ASTM D4060
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 66.0 °C
151 °F
Wet
93.0 °C
199 °F
Dry
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 32.0 °C
1.00 hour

@Temperature 89.6 °F
Tack Free
120 min

@Temperature 25.0 °C
2.00 hour

@Temperature 77.0 °F
Tack Free
150 min

@Temperature 32.0 °C
2.50 hour

@Temperature 89.6 °F
Light Load
180 min

@Temperature 16.0 °C
3.00 hour

@Temperature 60.8 °F
Tack Free
210 min

@Temperature 25.0 °C
3.50 hour

@Temperature 77.0 °F
Light Load
300 min

@Temperature 10.0 °C
5.00 hour

@Temperature 50.0 °F
Tack Free
420 min

@Temperature 16.0 °C
7.00 hour

@Temperature 60.8 °F
Light Load
540 min

@Temperature 10.0 °C
9.00 hour

@Temperature 50.0 °F
Light Load
960 min

@Temperature 32.0 °C
16.0 hour

@Temperature 89.6 °F
Full Load
1200 min

@Temperature 25.0 °C
20.0 hour

@Temperature 77.0 °F
Full Load
1800 min

@Temperature 32.0 °C
30.0 hour

@Temperature 89.6 °F
Full Chemical
2160 min

@Temperature 16.0 °C
36.0 hour

@Temperature 60.8 °F
Full Load
2160 min

@Temperature 25.0 °C
36.0 hour

@Temperature 77.0 °F
Full Chemical
2880 min

@Temperature 10.0 °C
48.0 hour

@Temperature 50.0 °F
Full Load
4320 min

@Temperature 16.0 °C
72.0 hour

@Temperature 60.8 °F
Full Chemical
5760 min

@Temperature 10.0 °C
96.0 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Grey