Chesterton ARC HT-S High Temperature Corrosion Resistant Coating

Category Polymer , Thermoset , Epoxy
Manufacturer Chesterton
Trade Name ARC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton ARC HT-S High Temperature Corrosion Resistant Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with conventional airless equipment. Spark testable, non-shrinking 100% solids. ARC HT-S is reinforced with high modulus reinforcements to improve long term resistance to cold wall induced blistering and delamination. Its unique chemistry allows for reliable long term immersion service at elevated temperatures without the need for post curing thereby simplifying installation. ARC HT-S is capable of in-situ curing. Benefits:High voltage spark testable to NACE SP 0188Capable of ambient cureTwo color system provides visual indicators of mixingAble to handle immersion in elevated temperature aqueous applications Suggested Uses:Process Cooling Water Heat ExchangersCrystallizers/EvaporatorsCentrifugesCondensate Return PumpsDistillation UnitsOil/Water, Oil/Gas Separator VesselsInformation provided by Chesterton
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Compressive Strength 106 MPa
15400 psi
ASTM D790
Adhesive Bond Strength >= 13.8 MPa
>= 2000 psi
ASTM D4541
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Wet Service
175 °C
347 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 32.0 °C
3.00 hour

@Temperature 89.6 °F
Overcoat Begin
240 min

@Temperature 25.0 °C
4.00 hour

@Temperature 77.0 °F
Overcoat Begin
240 min

@Temperature 32.0 °C
4.00 hour

@Temperature 89.6 °F
Tack Free
360 min

@Temperature 16.0 °C
6.00 hour

@Temperature 60.8 °F
Overcoat Begin
360 min

@Temperature 25.0 °C
6.00 hour

@Temperature 77.0 °F
Tack Free
480 min

@Temperature 10.0 °C
8.00 hour

@Temperature 50.0 °F
Overcoat Begin
480 min

@Temperature 16.0 °C
8.00 hour

@Temperature 60.8 °F
Tack Free
600 min

@Temperature 10.0 °C
10.0 hour

@Temperature 50.0 °F
Tack Free
720 min

@Temperature 32.0 °C
12.0 hour

@Temperature 89.6 °F
Overcoat End
1080 min

@Temperature 25.0 °C
18.0 hour

@Temperature 77.0 °F
Overcoat End
1440 min

@Temperature 16.0 °C
24.0 hour

@Temperature 60.8 °F
Overcoat End
1800 min

@Temperature 10.0 °C
30.0 hour

@Temperature 50.0 °F
Overcoat End
4320 min

@Temperature 32.0 °C
72.0 hour

@Temperature 89.6 °F
Full Mechanical
4320 min

@Temperature 32.0 °C
72.0 hour

@Temperature 89.6 °F
Full Chemical
5760 min

@Temperature 25.0 °C
96.0 hour

@Temperature 77.0 °F
Full Mechanical
5760 min

@Temperature 25.0 °C
96.0 hour

@Temperature 77.0 °F
Full Chemical
7200 min

@Temperature 16.0 °C
120 hour

@Temperature 60.8 °F
Full Mechanical
7200 min

@Temperature 16.0 °C
120 hour

@Temperature 60.8 °F
Full Chemical
8640 min

@Temperature 10.0 °C
144 hour

@Temperature 50.0 °F
Full Mechanical
8640 min

@Temperature 10.0 °C
144 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Blue
Gray