Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound

Category Ceramic , Polymer , Thermoset , Epoxy
Manufacturer Chesterton
Trade Name ARC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied by trowel or plastic applicator tool in one or two coats, as required. ARC HT-T is applied at a normal thickness of 900-1150 microns (35-45 mils). It is a 100% solids non-shrinking composite. ARC HT-T provides exceptional corrosion and erosion protection to high temperature equipment handling water solutions. The cured product also provides outstanding blister and abrasion resistance with a high gloss finishBenefits:Exceptional permeating and blister resistance in high temperature water applications, including mild acids and bases.High gloss surface reduces drag, improves flow and pump efficiencyTough resin structure resist thermal-mechanical shockOutstanding adhesion insures reliable performance with no undercutting or underfilm corrosionAdvanced reinforcement design provides outstanding abrasion resistanceAbility to in-service cure in static conditions reduces application costs and downtimeHigh voltage spark testable per NACE SP0188 Suggested Uses:CondensersHeat ExchangersPump VolutesPump ImpellersCondensate PumpsTanksValvesPressure VesselsHot Water PumpsDrill Mud Circulating EquipmentOil/Water SeparatorsOil Extraction ManifoldsCondensate TanksEvaporatorsSugar Process EquipmentInformation provided by Chesterton
Physical Properties Metric English Comments
Density 2.22 g/cc
0.0802 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
ASTM D2240
Elongation at Break 3.6 %
3.6 %
ASTM D638
Flexural Strength 53.8 MPa
7800 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Compressive Strength 93.1 MPa
13500 psi
ASTM D695
Adhesive Bond Strength 32.8 MPa
4760 psi
ASTM D4541
Impact Test 4.52 J
3.33 ft-lb
reverse; ASTM D2794
9.04 J
6.67 ft-lb
direct; ASTM D2794
Thermal Properties Metric English Comments
CTE, linear 30.2 µm/m-°C

@Temperature -5.00 - 25.0 °C
16.8 µin/in-°F

@Temperature 23.0 - 77.0 °F
ASTM E228
90.2 µm/m-°C

@Temperature 125 - 150 °C
50.1 µin/in-°F

@Temperature 257 - 302 °F
ASTM E228
Maximum Service Temperature, Air 110 °C
230 °F
Wet Service
150 °C
302 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 32.0 °C
3.00 hour

@Temperature 89.6 °F
Tack Free
180 min

@Temperature 32.0 °C
3.00 hour

@Temperature 89.6 °F
Overcoat Begin
240 min

@Temperature 25.0 °C
4.00 hour

@Temperature 77.0 °F
Tack Free
240 min

@Temperature 25.0 °C
4.00 hour

@Temperature 77.0 °F
Overcoat Begin
360 min

@Temperature 32.0 °C
6.00 hour

@Temperature 89.6 °F
Light Load
480 min

@Temperature 16.0 °C
8.00 hour

@Temperature 60.8 °F
Tack Free
480 min

@Temperature 16.0 °C
8.00 hour

@Temperature 60.8 °F
Overcoat Begin
540 min

@Temperature 25.0 °C
9.00 hour

@Temperature 77.0 °F
Light Load
1080 min

@Temperature 16.0 °C
18.0 hour

@Temperature 60.8 °F
Light Load
2160 min

@Temperature 32.0 °C
36.0 hour

@Temperature 89.6 °F
Service
2400 min

@Temperature 32.0 °C
40.0 hour

@Temperature 89.6 °F
Overcoat End
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Service
3120 min

@Temperature 25.0 °C
52.0 hour

@Temperature 77.0 °F
Overcoat End
4320 min

@Temperature 16.0 °C
72.0 hour

@Temperature 60.8 °F
Overcoat End
5040 min

@Temperature 16.0 °C
84.0 hour

@Temperature 60.8 °F
Service
Descriptive Properties Value Comments
Color Black
Green