Material Notes:
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand troweled on horizontal surfaces at a minimum thickness of 6 mm as well as poured into casting applications at minimum thickness of 9 mm (3/8”) or more. Non-shrinking, 100% solids. ARC MXC is formulated with a high concentration of ceramic beads and fine ceramic particles for extremely abrasive environments where superior protection is desirable. ARC MXC may be molded where close tolerances in application and a smooth finish are necessary, or where accessibility is limited. Benefits:Lowered viscosity allows it to be molded to precise dimensions for critical tolerances.Excellent wear characteristics extend equipment’s operating cycles.Tough resin structure resists thermal-mechanical shockPerforms well under fluctuation chemical environments. Suggested Uses:Exit ConesTransport Pipelines for Abrasive MaterialHoppers and SilosCyclonesCeramic Tile Lined ChutesSlurry Pumps and Pipe ElbowsInformation provided by Chesterton
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength at Break 29.0 MPa
4200 psi
ASTM D638
Elongation at Break 0.10 %
0.10 %
ASTM D638
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Flexural Modulus 4.83 GPa
701 ksi
ASTM D790
Compressive Strength 1100 MPa
159000 psi
ASTM D695
Adhesive Bond Strength 16.9 MPa
2450 psi
ASTM D4541
Impact Test 9.04 J
6.67 ft-lb
Direct; ASTM D2794
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 °C
203 °F
Wet Service
205 °C
401 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 32.0 °C
1.00 hour

@Temperature 89.6 °F
Tack Free
120 min

@Temperature 25.0 °C
2.00 hour

@Temperature 77.0 °F
Tack Free
150 min

@Temperature 32.0 °C
2.50 hour

@Temperature 89.6 °F
Light Load
180 min

@Temperature 16.0 °C
3.00 hour

@Temperature 60.8 °F
Tack Free
210 min

@Temperature 25.0 °C
3.50 hour

@Temperature 77.0 °F
Light Load
300 min

@Temperature 10.0 °C
5.00 hour

@Temperature 50.0 °F
Tack Free
420 min

@Temperature 16.0 °C
7.00 hour

@Temperature 60.8 °F
Light Load
540 min

@Temperature 10.0 °C
9.00 hour

@Temperature 50.0 °F
Light Load
960 min

@Temperature 32.0 °C
16.0 hour

@Temperature 89.6 °F
Full Load
1200 min

@Temperature 25.0 °C
20.0 hour

@Temperature 77.0 °F
Full Load
1980 min

@Temperature 32.0 °C
33.0 hour

@Temperature 89.6 °F
Full Chemical
2160 min

@Temperature 16.0 °C
36.0 hour

@Temperature 60.8 °F
Full Load
2400 min

@Temperature 25.0 °C
40.0 hour

@Temperature 77.0 °F
Full Chemical
2880 min

@Temperature 10.0 °C
48.0 hour

@Temperature 50.0 °F
Full Load
4800 min

@Temperature 16.0 °C
80.0 hour

@Temperature 60.8 °F
Full Chemical
6480 min

@Temperature 10.0 °C
108 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Blue