Material Notes:
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 14200Characteristics: Excellent Flexibility, Excellent Flow, Good Warping Resistance, Moderate Mold Release, Moderate ESCRApplications:Large Housewares, Tamper Evident Snap-On CapsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 190 °C
21 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength, Ultimate 11.2 MPa
1620 psi
ASTM D638
Tensile Strength, Yield 7.70 MPa
1120 psi
ASTM D638
Elongation at Break 540 %
540 %
ASTM D638
Flexural Modulus 0.124 GPa
18.0 ksi
3 pt. secant; ASTM D790
0.159 GPa
23.1 ksi
3 pt. Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Brittleness Temperature <= -72.0 °C
<= -97.6 °F
ASTM D746