Chevron Phillips 5570 LDPE High Clarity, Medium Impact Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5570 LDPE High Clarity, Medium Impact Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Good Optical Properties, Good Impact Strength, Excellent Processability, High Antiblock and Low SlipApplications:Baby Bottle LinersProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 1.3 g/10 min
1.3 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.210 GPa
30.5 ksi
ASTM D882
Secant Modulus, TD 0.230 GPa
33.4 ksi
ASTM D882
Coefficient of Friction 0.70
0.70
ASTM D1894
Dart Drop 2.50 g/micron
63.5 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 6.5 %
6.5 %
ASTM D2457
Gloss 65 %
65 %
at 45°. ASTM D 2457
105 %
105 %
at 60°. ASTM D 2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F