Material Notes:
DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practical toughness. Chevron EB6755 natural complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods.ApplicationsChevron EB6755 is particularly well suited for containers and lids used for packaging stress-crack aggressive food products (yot, sour cream, delicatessen salads, dips, etc.) and applications requiring excellent practical toughness such as multiple use lids.Information provided by Chevron Phillips Chemical Company.The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 3.2 g/10 min
3.2 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 81
81
ASTM D785
Tensile Strength at Break 17.9 MPa
2600 psi
at 2.0 in/min, Tested using a 50 mil. Sheet; ASTM D638
Tensile Strength, Yield 17.9 MPa
2600 psi
at 2.0 in/min, Tested using a 50 mil. sheet; ASTM D638
Elongation at Break 85 %
85 %
Tested using a 50 mil. Sheet; ASTM D638
Tensile Modulus 1.65 GPa
240 ksi
Tested using a 50 mil. Sheet; ASTM D638
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
1/4 in. at 73°F; ASTM D256
1.17 J/cm
2.20 ft-lb/in
1/8 in.; ASTM D256
0.694 J/cm

@Temperature -17.8 °C
1.30 ft-lb/in

@Temperature 0.000 °F
0.125 in (3.2 mm) sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Unannealed specimen; ASTM D648
Vicat Softening Point 102 °C
215 °F
ASTM D1525