Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Gas Phase Linear Hexene CopolymerASTM D 4976 Classification: PE 235, A 54607ASTM D3350 Classification: 335540AApplications: Base resin for use in utility and conduit pipe applications.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F<sub>0-</sub>; ASTM D1693
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
1% Secant; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746