Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on fast production cycles and are easily processed by injection molding. This resin can be tinted or colored in a variety of transparent and opaque shades. Compared to BK10, BK15 offers improved mold release with the same injection molding process conditions and equivalent molded part performance and properties. Molded parts offer excellent clarity, good toughness, good stiffness, and high surface gloss.Applications: Major applications include molded boxes and containers, toys, displays, medical devices, overcaps, and novelties.Processing Recommendations:Injection Molding: Minimum melt temperature between 193-232°C necessary to permit mold fill. Minimum injection pressure required to fill the cavity. Maximum back pressure of 0.3 MPa. Drying: Generally, no need to dry resin.Specification Data: FDA Regulations 21 CFR 177.1640; suitable for contact with non-fatty foods. [parts over 0.200 inches thick, for alcoholic beverages, or for high temperature food use (hot filled over 150°F or heat sterilized over 212°F) would require additional testing]Data provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 200 °C
15 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 21.4 MPa
3100 psi
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 200 %
200 %
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 31.7 MPa
4600 psi
Test specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 1.482 GPa
214.9 ksi
Test specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Impact Test 29.7 J

@Thickness 3.17 mm
21.9 ft-lb

@Thickness 0.125 in
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Vicat Softening Point 80.0 °C
176 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 193 - 232 °C
379 - 450 °F
Injection