Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips MarFlex® 1125 Polyethylene; LDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 1125 Polyethylene; LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typical blown film applications include: LinersTrash bagsConverter filmsInformation provided by Phillips
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D-1505
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
Blown Film at 1.25 mil; ASTM F-1249
Oxygen Transmission Rate 5200 cc/m²/day
335 cc/100 in²/day
Blown Film at 1.25 mil; ASTM D-3985
Melt Index of Compound 2.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Antiblock Level 4000 ppm
4000 ppm
Slip Level 0.00 ppm
0.00 ppm
Mechanical Properties Metric English Comments
Coefficient of Friction 0.55
0.55
Blown Film at 1.25 mil; ASTM D-1894
Elmendorf Tear Strength, MD 4.92 g/micron
125 g/mil
Blown Film at 1.25 mil; ASTM D-1922
Elmendorf Tear Strength, TD 3.94 g/micron
100 g/mil
Blown Film at 1.25 mil; ASTM D-1922
Dart Drop 3.15 g/micron
80.0 g/mil
Blown Film at 1.25 mil; ASTM D-1709
Thermal Properties Metric English Comments
Melting Point 107 °C
225 °F
ASTM D-3418
Vicat Softening Point 96.0 °C
205 °F
ASTM D-1525
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
Blown Film at 1.25 mil; ASTM D-1003
Gloss 80 %
80 %
60°, Blown Film at 1.25 mil; ASTM D-2457
Users viewing this material also viewed the following: