Chevron Phillips MarFlex® 5428 LDPE Cast Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 5428 LDPE Cast Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Excellent OpenabilitySuited for high speed convertingGood clarityLow COFApplications: Bakery FilmBreak BagsInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
Base Density; ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Index of Compound 2.2 g/10 min
2.2 g/10 min
ASTM D1238E
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.159 GPa
23.1 ksi
ASTM D882
Secant Modulus, TD 0.165 GPa
23.9 ksi
ASTM D882
Coefficient of Friction 0.10
0.10
ASTM D1894
Dart Drop 3.12 g/micron
79.2 g/mil
1.5" Dart, 26" Drop Height; ASTM D1709
Optical Properties Metric English Comments
Haze 6.5 %
6.5 %
ASTM D1003
Gloss 75 %
75 %
45°; ASTM D2457
115 %
115 %
60°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 260 °C
500 °F
Die Opening 0.0635 cm
0.0250 in
Extruder Size 6.35 cm
2.50 in
Descriptive Properties Value Comments
Antiblock Very High
Slip High
Copyright © lookpolymers.com All Rights Reserved