Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Linear Homopolymer; ASTM D 4976 Classification: PE 243, A 63700Characteristics: Moderate Flow, Good Impact Strength, Excellent Stiffness, Good ESCR, Moderate Shrinkage ResistanceApplications:Crates and totes, structural foamData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
High Load Melt Index 216 g/10 min

@Load 21.6 kg,
Temperature 190 °C
216 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
3 pt. secant. ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525