Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HMN 55180 Polyethylene, Injection Molding Grade, HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HMN 55180 Polyethylene, Injection Molding Grade, HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Meets FDA Regulation 177.1520. Excellent impact strength and warpage resistance; high surface gloss.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 125 %
125 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Electrical Properties Metric English Comments
Dielectric Constant 2.33

@Frequency 100000 Hz
2.33

@Frequency 100000 Hz
ASTM D1531
Dielectric Strength 20.0 kV/mm

@Thickness 3.17 mm
508 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor >= 0.00010

@Frequency 100000 Hz
>= 0.00010

@Frequency 100000 Hz
ASTM D1531
Processing Properties Metric English Comments
Processing Temperature 204 - 260 °C
399 - 500 °F
Stock Temperature