Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density PolyethyleneCustomer Benefits: This extra high molecular weight polyethylene is tailored for large containers with exhibit outstanding impact and creep resistance, excellent ESCR, and excellent chemical resistance.Applications: DrumsProcessing Recommendations:To ensure optimum part quality, maintain a stock temperature of 193-210°C.Specification Data: ASTM D1248-Type III, Class A, Category 5Property Comments: Physical Properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928.Data provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 1000 hour
1000 hour
Condition A, F<sub>50</sub>, Condition B: 1000; ASTM D1693
Melt Flow 5.5 g/10 min
5.5 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
2 in per min; ASTM D638, Type IV
Elongation at Break 600 %
600 %
2 in per min; ASTM D638, Type IV
Flexural Modulus 1.28 GPa
186 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746