Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS); Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyphenylene Sulfide CompoundRyton® PR09-60 is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI UnitsData provided by Chevron Phillips Chemical Company LP.Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 95.0 MPa
13800 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Unnotched 13.0 J/cm
24.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
29.4 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ASTM E831
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistance 1.00e+12 ohm

@Temperature 90.0 °C
1.00e+12 ohm

@Temperature 194 °F
95% RH, 48 hrs
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
ASTM D150
3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
610 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 50 sec
50 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
UL 746A